Polymer Property : Izod Impact, Notched = 3.41696 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.41696 - 3.41696 J/cm

@Temperature -40.0 - -40.0 °C
6.40137 - 6.40137 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 3.42 J/cm Grade Count:2
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Izod Impact, Notched 0.170 - 3.41696 J/cm

@Temperature -20.0 - 4.00 °C
0.318 - 6.40137 ft-lb/in

@Temperature -4.00 - 39.2 °F
Average value: 1.07 J/cm Grade Count:8
Overview of materials for Polypropylene, Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Blow Molding Grade". Each property range of values reported is minimum and maximum values..