Polymer Property : Izod Impact, Notched = 3.77 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.01 J/cm

@Temperature 23.0 °C
3.77 ft-lb/in

@Temperature 73.4 °F
ASTM D256
IRPC Polimaxx Polene 2511HX GA5 Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 25% GLASS FIBRE REINFORCED VERY HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, LOW SHRINKAGE, HIGH STIFFNESS, CONTAIN UV STABILIZER AND LONG TERM..