Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.05 J/cm | 3.84 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific) Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Izod Impact, Notched | 2.05 J/cm | 3.84 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X2420 PC+POLYESTER (Asia Pacific) Xenoy*X2420 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and impact strength. X2420 has enhanced melt flowability, impact ductility and broad co.. |