Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.39 J/cm @Thickness 3.17 mm |
4.48 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |
|||
Izod Impact, Notched | 2.39 J/cm | 4.48 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON RX00327 PA 66 LNP* VERTON* RX00327 is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this material is: Structural. |