Mechanical Properties Metric English Comments
Izod Impact, Notched 4.69 J/cm

@Thickness 4.00 mm,
Temperature 23.0 °C
8.79 ft-lb/in

@Thickness 0.157 in,
Temperature 73.4 °F
ISO 180
Azdel Plus C401-B01 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope..