Mechanical Properties Metric English Comments
Izod Impact, Notched 24.0 J/cm
45.0 ft-lb/in
Owens Corning Glass Fiber Reinforced Epoxy (Filament Wound), 80 wt.% glass
Epoxies are highly resistant to water, alkalis and organic solvents. Although standard epoxies have only a fair resistance to acids and oxidizing agents, they can be formulated for better resistance..