Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.78 J/cm | 5.20 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hysun™ 697 ASA Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Izod Impact, Notched | 2.78 - 3.84 J/cm | 5.20 - 7.20 ft-lb/in | |
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr.. |