Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.47 J/cm | 10.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Izod Impact, Notched | 5.47 J/cm | 10.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Izod Impact, Notched | 5.47 J/cm | 10.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |