Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman 310 Utility Black PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman 330 White PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman 380 Grey PC/ABS Alloy Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum.. |
|||
Izod Impact, Notched | 4.00 - 5.61 J/cm @Thickness 3.17 mm |
7.50 - 10.5 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Shuman FR380 Grey PC/ABS Alloy, Flame Retardant Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum.. |