Mechanical Properties Metric English Comments
Izod Impact, Notched 3.12 J/cm
5.85 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer
LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant.