Mechanical Properties
Metric
English
Comments
Izod Impact, Notched
3.44
J/cm
6.44
ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP 2F006 ETFE
LNP* THERMOCOMP* 2F006 is a compound based on ETFE containing 30% Glass Fiber.