Polymer Property : Izod Impact, Notched = 6.90 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.641 - 3.68 J/cm
1.20 - 6.90 ft-lb/in
Average value: 1.76 J/cm Grade Count:14
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Izod Impact, Notched 0.427 - 3.68 J/cm
0.800 - 6.90 ft-lb/in
Average value: 1.51 J/cm Grade Count:86
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..