Polymer Property : Izod Impact, Notched = 7.95 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 7.95 J/cm
14.9 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® CY6414 PC (Asia Pacific)
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer
Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Asia Pacific)
Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Asia Pacific)
Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with ..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with ..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific)
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer
Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific)
Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Asia Pacific)
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HPX4EU PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific)
Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HPX4REU PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer
Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) ..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Asia Pacific)
Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) ..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Europe-Africa-Middle East)
Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) ..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® FXD1413T PC Copolymer (Asia Pacific)
Clear PC-siloxane copolymer with excellent processability, in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may af..
Izod Impact, Notched 7.95 J/cm
14.9 ft-lb/in
ASTM D256
KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet
Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakage..
Izod Impact, Notched 7.95 J/cm

@Temperature -30.0 °C
14.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer
Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with ..