Mechanical Properties Metric English Comments
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 1100-25 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 1200H-15 Polyester SMC
Premi-Glas® 1200H-15 is a 15% fiberglass-reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94 HB flame re..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 1240-15 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 1240-15 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC
Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 2103-22 CRSX Polyester BMC
Premi-Glas® 2103-22 CR-SX is a 22% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 2103-22 CR-SX-HT Fiberglass Reinforced Thermoset BMC
Premi-Glas® 2103-22 CR-SX-HT is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL ..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
Premix Premi-Glas® 3101-20 Polyester BMC
Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-..
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.
Izod Impact, Notched 4.25 J/cm
7.96 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-LOY AX11421 ABS