Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.02 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Asia Pacific) Blow moldable, impact modifed XENOY |
|||
Izod Impact, Notched | 8.02 J/cm | 15.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X6800BM PBT (Europe-Africa-Middle East) Blow moldable, impact modifed XENOY |