Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.06 J/cm | 15.1 ft-lb/in | |
Kraton® G1730 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |