Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.28 J/cm | 15.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer Improved flow PC with excellent processability and mold release. |
|||
Izod Impact, Notched | 8.28 J/cm | 15.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 143X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |
|||
Izod Impact, Notched | 8.28 J/cm | 15.5 ft-lb/in | NB; ASTM D256 |
LyondellBasell SEQUEL® E3000 FR TPO Description: SEQUEL® E3000FR thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spe.. |
|||
Izod Impact, Notched | 8.28 J/cm @Temperature 22.8 °C |
15.5 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 8.28 J/cm @Temperature 22.8 °C |
15.5 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol 6608-L Nylon 66, High Impact Modified, Lubricated Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 8.28 J/cm @Temperature 22.8 °C |
15.5 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol 6608-L UV Black Nylon 66, High Impact Modified, Lubricated, UV Stable Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 8.28 J/cm | 15.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |