Mechanical Properties Metric English Comments
Izod Impact, Notched 0.300 - 8.54 J/cm
0.562 - 16.0 ft-lb/in
Average value: 1.04 J/cm Grade Count:119
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched 7.47 - 8.54 J/cm
14.0 - 16.0 ft-lb/in
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie..
Izod Impact, Notched 6.41 - 8.54 J/cm
12.0 - 16.0 ft-lb/in
Bulk Molding Compounds BMC 1410 Electrical Grade
BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally..