Polymer Property : Izod Impact, Notched = 8.59 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 8.59 J/cm

@Temperature -20.0 °C
16.1 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched 8.59 J/cm

@Temperature -20.0 °C
16.1 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched 8.59 J/cm

@Temperature -20.0 °C
16.1 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Europe-Africa-Middle East)
11 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched 8.59 J/cm

@Temperature -20.0 °C
16.1 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only
Izod Impact, Notched 8.59 J/cm

@Temperature -20.0 °C
16.1 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized
Izod Impact, Notched 8.59 J/cm
16.1 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comtuf® 602 Nylon 6/6, High Impact Modified
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Izod Impact, Notched 8.59 J/cm

@Temperature -20.0 °C
16.1 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Europe-Africa-Middle East)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized, available in transparent colors only
Copyright © lookpolymers.com All Rights Reserved