Polymer Property : Izod Impact, Notched = 8.99 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 8.99 J/cm

@Temperature -30.0 °C
16.8 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer
Izod Impact, Notched 8.99 J/cm

@Temperature -30.0 °C
16.8 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Europe-Africa-Middle East)
7 MFR LEXAN HFD Copolymer
Izod Impact, Notched 8.99 J/cm

@Temperature -30.0 °C
16.8 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Izod Impact, Notched 8.99 J/cm

@Temperature -30.0 °C
16.8 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Izod Impact, Notched 8.99 J/cm

@Temperature -30.0 °C
16.8 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East)
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Izod Impact, Notched 8.99 J/cm

@Temperature -30.0 °C
16.8 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer
7 MFR LEXAN HFD Copolymer