Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.02 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD104R PC FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Izod Impact, Notched | 9.02 J/cm @Temperature 23.0 °C |
16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML6819 PC (Asia Pacific) Medium flow, UV stabilised, high impact grade of polycarbonate.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 9.02 J/cm | 16.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Izod Impact, Notched | 9.02 J/cm | 16.9 ft-lb/in | Method B; Ductile Failure |
Elastomer Engineering Elastamide 200 Elastomer Modified RIM Nylon 6 26% crystallinity. Information supplied by Elastomer Engineering. |
|||
Izod Impact, Notched | 9.02 J/cm | 16.9 ft-lb/in | ASTM D256 |
Aclo Accucomp Polycarbonate POL051L Medium Viscosity |