Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 101R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 101R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. Internal mold release. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 103 PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 103R PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 104 PC UL rated HB. 200 series recommended when V-2 rating required. 7.0 MFR, for thicker sections without sinks. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 104 PC (Asia Pacific) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 131 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 131R PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
Izod Impact, Notched | 9.07 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 133 PC (Asia Pacific) Nonhalogenated. 3.5 MFR. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 134R PC Nonhalogenated. 3.5 MFR. Internal mold release. FDA food contact compliant in limited colors. |
|||
Izod Impact, Notched | 9.07 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 135 PC General purpose low flow polycarbonate powder gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 201 PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 203R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPS6 PC (Europe-Africa-Middle East) Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LS3 PC (Asia Pacific) Automotive lens applications. Medium-high viscosity. UV-stabilized. Adhesion to coatings. Transparent colors only. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® OQ2720 PC Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent production control conditions. |
|||
Izod Impact, Notched | 9.07 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXE101R PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 200 10 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 200 6 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 2060 10 Polycarbonate, Sterilization Grade CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 300 10 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 300 6 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 103R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release... |
|||
Izod Impact, Notched | 9.07 J/cm @Temperature 23.0 °C |
17.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXE101 PC Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). 7.0 MFR, for thicker sections without sinks.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 9.07 J/cm | 17.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SD1318 PC High viscosity, UV stabilized multi purpose grade. |