Mechanical Properties Metric English Comments
Izod Impact, Notched 1.91 - 5.12544 J/cm

@Temperature -40.0 - 121 °C
3.58 - 9.60205 ft-lb/in

@Temperature -40.0 - 250 °F
Average value: 1.85 J/cm Grade Count:3
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..