Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.76 - 5.33 J/cm | 3.30 - 9.99 ft-lb/in | Average value: 3.80 J/cm Grade Count:66 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |