Charpy Impact, Notched 0.310 J/cm²

@Temperature 23.0 °C
1.48 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® S CV300 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Charpy Impact, Notched 0.310 J/cm²

@Temperature -30.0 °C
1.48 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® K224-HG2U (Cond.) 10% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Charpy Impact, Notched 0.310 J/cm²

@Temperature -30.0 °C
1.48 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Solvay TECHNYL® C 52G1 V20 PA6, DRY
Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer..