Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.440 J/cm² @Temperature -30.0 °C |
2.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Charpy Impact, Notched | 0.440 J/cm² @Temperature 23.0 °C |
2.09 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Novamid® 1010C2 PA6 Easy Molding Grade |
|||
Charpy Impact, Notched | 0.440 J/cm² @Temperature 23.0 °C |
2.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |