Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 0.670 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.670 J/cm²

@Temperature 23.0 °C
3.19 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre
FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben..
Charpy Impact, Notched 0.670 J/cm²

@Temperature 23.0 °C
3.19 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A 35E 990 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..