Polymer Property : Charpy Impact, Notched = 0.904 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.190 J/cm²

@Temperature 23.0 °C
0.904 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating
Borcoat™ MA115E is a highly filled polypropylene compound and is self colored. Applications: Borcoat™ MA115E is recommended as heavy weight coating for special applications used in steel pipe coa..