Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 GF 50 Polyamide 66, 50% Glass Fiber FeaturesChemically reinforced with 50% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 945ASR PC Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE161R PC (Europe-Africa-Middle East) LEXAN FXE161R is a transparent/translucent medium viscosity grade for special effects with fluorescent appearance. Color package may affect performance. LEXAN FXE161R contains a release agent to ens.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® GLX143 PC (Europe-Africa-Middle East) Lexan* GLX resin is a medium viscosity grade which is an excellent candidate for applications with high optical quality requirements, such as automotive glazing applications. Available in transparen.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC T2020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3840 MO 40% Glass Filled Polypropylene Copolymer INNOPOL® CS 2-3840 MO is a 40 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-3840 MO is recommended for p.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -40.0 °C |
6.66 ft-lb/in² @Temperature -40.0 °F |
ISO 179-1eA |
Lanxess Durethan® AKV 50 H3.0 000000 Nylon 66, 50% Glass Fibers PA 66, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Terluran® EGP-7 ABS Terluran EGP-7 is an extrusion grade with well balanced properties.UL 94 HBInformation provided by Styrolution |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Total PPC 8780 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 8780 is a controlled rheology heterophasic copolymer with a Melt Flow index of 18 g/10 min.Polypropylene PPC 8780 has been specially developed for the injection molding of lids com.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K224-HG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® TV8 260 PBT-30% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® TE351 PA46 FR(17) Flame Retardant, Heat Stabilized |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® PLUS PLS95G35DH1 BK031 Nylon Zytel® PLS95G35DH1 BK031is a high flow 35% glass reinforced PA using SHIELD Technology, only from DuPont, combining excellent surface appearance, excellent welding and fatigue retention, exceptiona.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, Conditioned Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
6.66 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PQ 83 T 40 PP, 40% mineral filling FeaturesModified PP for injection moulding with the content of 40% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased .. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -20.0 °C |
6.66 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPHC EP1001F Polypropylene Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® FXE144H PC (Europe-Africa-Middle East) FXE144H is a Lexan PC Translucent Grade in our VisualFX Portfolio. It is part of Energy family, which includes Illuminate, Glass, and Flame effects. Grade was developed to meet the Aesthetic Differe.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature -30.0 °C |
6.66 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® PB581-H Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 1.40 J/cm² @Temperature 23.0 °C |
6.66 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |