Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.50 J/cm² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYblend 65FS PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYblend 85H PC/ABS-Blend Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.50 J/cm² @Thickness 102 mm, Temperature 23.0 °C |
11.9 ft-lb/in² @Thickness 4.00 in, Temperature 73.4 °F |
ISO 179 |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® FXC810AL PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Alpine White colour effects. The colour package may effect performance.This data was.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® FXC813SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC813SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC813SK is suitable for those applications that require sparkl.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 HI HV TS PA6 with impact modifier PA 6 higher viscosity, heat stabilized, impact modified for extrusion and blow molding. Automotive applications as air ducts and fuel filter pipes, fuel and oil containers.Information Provided by Pl.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP TOUCH 25325 Polypropylene, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -20.0 °C |
11.9 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PP TOUCH 25325 R3 Polypropylene, Glass Fiber Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-PG2U (Cond.) 13% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued ** Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® S223-TP4 Impact Modified Nylon 66 (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-G3U (Cond.) 15% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-PG2U (Cond.) 13% Glass Reinforced, Impact Modified Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -40.0 °C |
11.9 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
Kuraray Genestarâ„¢ N1006D-H31 Nylon Standard unreinforced extrusion grade. Main Features:Chemical resistanceLong term heat resistanceExample of applications:Tube applications |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Lanxess Pocan® S 1506 000000 PBT PBT, non-reinforced, injection molding extrusion, impact modified |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BKV 50 H2.0 901510 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 12.0 °C |
11.9 ft-lb/in² @Temperature 53.6 °F |
ISO 179/1eA |
Styron CALIBREâ„¢ 303-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K223-TP4 Impact Modified Nylon 6 (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-PG6 Impact Modified Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K240-HPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
DIN EN ISO 179 |
BASF Elastollan C 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, Conditioned Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K-FHG0 (Cond.) 50% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® R633H Nylon 66/6, 33% Glass Reinforced, Conditioned Vydyne® R633H is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in natural, this injection-molding grade resin is lubricated for machine feed and mold .. |
|||
Charpy Impact, Notched | 2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, Conditioned Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |