Polymer Property : Charpy Impact, Notched = 12.5 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 12.5 J/cm²

@Temperature 23.0 °C
59.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
DSM Stanyl® TW363 Nylon 46 (European Grade) (Cond)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..