Mechanical Properties Metric English Comments
Charpy Impact, Notched 184.7 J/cm²

@# of Cycles 1.00 ,
Temperature -17.8 °C
879.0 ft-lb/in²

@# of Cycles 1.00 ,
Temperature 0.000 °F
Longitudinal
AK Steel NITRONIC® 19-D Duplex Stainless Steel
AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}), good drawing and welding characteristi..