Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.590 J/cm²

@Temperature -30.0 °C
2.81 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A RV150 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..