Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 5.60 J/cm² @Temperature 23.0 °C |
26.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 65CI PC/ABS-Blend Information provided by Polykemi AB |