Mechanical Properties Metric English Comments
Charpy Impact, Notched 29.0 J/cm²

@Temperature 500 °C
138 ft-lb/in²

@Temperature 932 °F
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki..
Charpy Impact, Notched 29.0 J/cm²

@Temperature 300 °C
138 ft-lb/in²

@Temperature 572 °F
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki..
Charpy Impact, Notched 29.0 J/cm²

@Temperature 23.0 °C
138 ft-lb/in²

@Temperature 73.4 °F
International Mold Steel DH2F Pre-Hardened H13-Type Mold Steel
Description: DH2F is one of the best machining pre-hardened H13-type steels available.Unique Characteristics: 38-42 HRc hardness.Through hardened for exceptional dimensional stability.Cuts mold maki..