Polymer Property : Charpy Impact, Notched = 4.30 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.903 J/cm²

@Temperature 0.000 °C
4.30 ft-lb/in²

@Temperature 32.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BMU130P Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Asia Paci..
Charpy Impact, Notched 0.903 J/cm²

@Temperature -20.0 °C
4.30 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap..
Charpy Impact, Notched 0.903 J/cm²

@Temperature 22.8 °C
4.30 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CNU 012 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive applications. Availability: Africa & Middle East, Asia Pacific, Europe, South America and Nor..
Charpy Impact, Notched 0.903 J/cm²

@Temperature 22.8 °C
4.30 ft-lb/in²

@Temperature 73.0 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CNW 010 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior trim applications requiring low warpage.Availability: Africa & Middle East, Asia Pac..