Polymer Property : Charpy Impact, Notched = 43.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 9.05 J/cm²

@Temperature 23.0 °C
43.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Solvay TECHNYL® A 258 PA Black 2N PA66, DRY
Description: Unreinforced and modified polyamide 66, UV and thermal stabilized with excellent impact resistance, for injection molding.Available in: Europe Product Applications: TECHNYL® A 258P1 ..