Mechanical Properties Metric English Comments
Charpy Impact, Notched 5.10 J/cm²

@Temperature 23.0 °C
24.3 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PC 71 T 15 PP, 15% mineral filling
FeaturesModified PP for injection moulding with the content of 15% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches - pack..
Charpy Impact, Notched 5.10 J/cm²

@Temperature 23.0 °C
24.3 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PQ 83 T 15 PP, 15% mineral filling, UV stabilization
FeaturesModified PP for injection moulding with the content of 15% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased ..
Charpy Impact, Notched 5.10 J/cm²

@Temperature 23.0 °C
24.3 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PC 93 T 5 PP reinforced with 5% mineral filler
Features: Modified PP for injection moulding with the content of 5% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. General application in all industry branches.Packa..