Polymer Property : Charpy Impact, Notched = 6.70 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.41 J/cm²

@Temperature 0.000 °C
6.70 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
ExxonMobil PP8013L1 Polypropylene Impact Copolymer
Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t..