Charpy Impact, Notched 1.62 J/cm²

@Temperature 23.0 °C
7.71 ft-lb/in²

@Temperature 73.4 °F
DAM; ISO 179/1eA
DuPont Performance Polymers Zytel® 74G33W NC010 Nylon 66  (Unverified Data**)
Zytel® 74G33W NC010 is a 33% glass reinforced nylon 66 and nylon 6 co-melt resin with improved weatherability.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 1.62 J/cm²

@Temperature 23.0 °C
7.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax BFG30-FH00N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.