Polymer Property : Charpy Impact, Notched = 9.50 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXRL0662 PC
Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. ..
Charpy Impact, Notched 9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1A
Gromax ATE90-FN01N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact, Notched 9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
partial break; 50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610  (Unverified Data**)
Zytel® RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is a black, unreinforced, toughened and heat stabilised r..
Charpy Impact, Notched 9.50 J/cm²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
partial break; 50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610  (Unverified Data**)
Zytel® RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by weight. It is an unreinforced and toughened resin for injection molding..