Polymer Property : Charpy Impact Unnotched = 0.790 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.790 J/cm²

@Temperature 23.0 °C
3.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/1eU
FKuR Kunststoff Fibrolon® P 7550 Wood-Plastic Compound, Fiber Reinforced
FIBROLON® are fiber reinforced compounds. Fibrolon® P 7550 has a polypropylene base. With the brand name of FIBROLON® FKuR has developed natural fiber reinforced compounds (Wood-Plastics-C..