Polymer Property : Charpy Impact Unnotched = 1.34 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.34 J/cm²
6.38 ft-lb/in²
ISO 179-1
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic
Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by ..