Polymer Property : Charpy Impact Unnotched = 1.42 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.42 J/cm²
6.76 ft-lb/in²
EN ISO 179
Ensinger TECASINT™ 2031 Polyimide, 40% Graphite Filled (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...