Mechanical Properties Metric English Comments
Charpy Impact Unnotched 8.70 - 103 J/cm²

@Temperature -30.0 - -30.0 °C
41.4 - 490 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 68.3 J/cm² Grade Count:6
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum ..