Polymer Property : Charpy Impact Unnotched = 12.5 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 12.5 J/cm²

@Temperature 23.0 °C
59.5 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment
PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS.
Charpy Impact Unnotched 12.5 J/cm²
59.5 ft-lb/in²
ISO 179
Styrolution Terluran® GP-35 ABS
Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an..
Charpy Impact Unnotched 12.5 J/cm²
59.5 ft-lb/in²
dry; ISO 179
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene
Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH.
Charpy Impact Unnotched 12.5 J/cm²
59.5 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60
Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory..
Charpy Impact Unnotched 12.5 J/cm²

@Temperature -30.0 °C
59.5 ft-lb/in²

@Temperature -22.0 °F
BASF Procom® X10S 773 Polypropylene
Car bumpers and spoilers where good paintability is required.Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 12.5 J/cm² - NB
59.5 ft-lb/in² - NB
Average value: 18.9 J/cm² Grade Count:15
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Charpy Impact Unnotched 12.5 J/cm²
59.5 ft-lb/in²
dry; ISO 179/1eU
EMS-Grivory Grivory® BM-30/2 PA6-MD30
Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App..
Charpy Impact Unnotched 12.5 J/cm²

@Temperature 30.0 °C
59.5 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® BM-30/2 PA6-MD30
Product description: Grilon BM-30/2 is a 30% mineral reinforced PA6 injection molding grade. Grilon BM-30/2 has the following important properties: Iow warpageImpact resistantIsotropic shrinkage App..