Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | ISO 179/1eU |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree.. |
|||
Charpy Impact Unnotched | 13.0 - 1000 J/cm² | 61.9 - 4760 ft-lb/in² | Average value: 16.3 J/cm² Grade Count:29 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | |
Polimeri Europa SINKRAL C350 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-08-16-25 Heat resistant injection moulding grade. Combines good flow with toughness and high thermal charac.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | |
Polimeri Europa SINKRAL PD M323 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose injection moulding grade that exhibits outstanding flow and thermal stability duri.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 6-7834 Polyamide 12, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Dynamic stressed parts.Low waterabsorbtion, for dimensional stable precision parts.Isotropic sh.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Forsan® 449 Acrylonitrile Butadiene Styrene (ABS) High flow, high gloss, suitable for electroplating.Applications: General purpose, intricate and thin-walled productsHousehold appliances, vacuum cleaners, heels, toys, fan grilles, etc.Synthos was f.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 50H1 PA66, DRY Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | Type 1, Edgewise; ISO 179 |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA), 60% Glass Fiber Amodel® A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional .. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-50/2 PA6-I-GF50 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® LKN-5H PA12-GB50 Product description: Grilamid LKN-5H is a 50% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | |
BASF Novolen® 1040 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | |
BASF Novolen® 1101 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature -30.0 °C |
61.9 ft-lb/in² @Temperature -22.0 °F |
|
BASF Polystyrol® 476 L Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade. When extruded it is often mixed with PS 165 H.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | ISO 179 |
BASF Ultramid® 8260 HS BK-102 40% Mineral Filled PA6 (Dry) Ultramid 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced PA6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined wi.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Charpy Impact Unnotched | 13.0 J/cm² | 61.9 ft-lb/in² | |
BASF Novolen® 1102 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 13.0 J/cm² @Temperature 23.0 °C |
61.9 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 900P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing thermal stability.Information provided by DuPont Perform.. |