Mechanical Properties Metric English Comments
Charpy Impact Unnotched 14.2 - 15.4 J/cm²

@Temperature -30.0 - -30.0 °C
67.6 - 73.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 14.8 J/cm² Grade Count:2
Overview of materials for Nylon 11 with Graphite Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 14.2 J/cm²

@Temperature -30.0 °C
67.6 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Dry)
Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good ..