Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® LUX7189 PC (Europe-Africa-Middle East) Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Lexan® LUX7189 PC (Europe-Africa-Middle East) Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems. |
|||
Charpy Impact Unnotched | <= 16.0 J/cm² @Temperature -30.0 - -30.0 °C |
<= 76.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 14.0 J/cm² Grade Count:2 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | |
Polimeri Europa SINKRAL G320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1e |
Aardvark Polymers AARTEL® 850IM Rotational Molding Resin Aartel 850 IM is a moderately toughened impact modified acetal copolymer which exhibits ductility in bending and impact loading. The ductile, rather than brittle, failure mode gives designers more f.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® H801 High heat resistance, PC modified, low emission, increased flow.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | 63.5 HRC |
International Mold Steel Daido DRM3 Matrix High-Speed Steel This conventional grade MH88 has been improved to DRM3. High hardness and tough DRM3 with excellent hardenability is suitable for high precision cold working tools.Information provided by Internatio.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature 23.0 °C |
76.1 ft-lb/in² @Temperature 73.4 °F |
80x10x4mm; ISO 179/1eU |
SYNTHOS Forsan® 573 L Acrylonitrile Butadiene Styrene (ABS) Increased heat resistant, glossy, UV stabilized.Applications: Electrotechnics, automotiveHousehold appliances, office equipment, car interior parts, profiles, ABS sheets, etc.Synthos was formerly kn.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | ISO 179 |
Styrolution Terblend® N 3158 ASA / PA, 9% Mineral filled Terblend® N 3158 is an 9% mineral-filled ABS/PA blend with good dimensional stability, enhanced rigidity and excellent heat resistance, so that this grade can be applied for online-painting.High .. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | ISO 179/1eU |
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AL is a medium viscosity acetal homopolymer with an advanced system of lubrication for applications requiring .. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² @Temperature -30.0 °C |
76.1 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG500AL is a medium viscosity acetal homopolymer lubricated for low wear .. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | |
BASF Novolen® 2248 TC Polypropylene Nucleated grade with antistatic agent for injection moldings.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 16.0 J/cm² | 76.1 ft-lb/in² | |
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe) Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF. |