Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.80 - 3.80 J/cm² @Temperature -20.0 - -20.0 °C |
18.1 - 18.1 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 3.80 J/cm² Grade Count:1 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 3.80 - 3.80 J/cm² @Temperature -30.0 - -30.0 °C |
18.1 - 18.1 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.80 J/cm² Grade Count:1 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |